written 8.7 years ago by |
Material Science & Metallurgy - Jan 2013
Mechanical Engineering (Semester 3)
TOTAL MARKS: 100
TOTAL TIME: 3 HOURS
(1) Question 1 is compulsory.
(2) Attempt any four from the remaining questions.
(3) Assume data wherever required.
(4) Figures to the right indicate full marks.
1 (a) Define atomic packing factor and calculate atomic radius and packing factor for BCC structure (8 marks)
1 (b) With a neat sketch,expalin the line dislocation (6 marks)
1 (c) State and explain the fick's second law of diffusion.(6 marks)
2 (a) With the help of a neat schematic conventional stress diagram for mild steel under tension,explain clearly the behaviour of the material till fracture(6 marks)
2 (b) Expalin non-linear elastic properties when a material is subjected to static tension (6 marks)
2 (c) What is work hardening?Explain the reasons for the same(6 marks)
3 (a) Explain with neat figure ductile feature using both stress strain and stages of fracture (8 marks)
3 (b) What is mean by stress relaxation ?Explain with figure(6 marks)
3 (c) With the help of sketch,discuss the different types of stress cycles which bring about fatigue failure(6 marks)
4 (a) Explain with neat sketches the different stages of mechanism of solidification (8 marks)
4 (b) Define solid solution .Explain the substitutional and interstiatial solid solution (8 marks)
4 (c) Explain the factor governing the formation of substitutional solid solution(4 marks)
5 (a) Draw and explain the Iron -Iron carbide equilibrium diagram and label all the points and field (10 marks)
5 (b) Consruct a phase digram using the following data and label all the fields ;
Melting point of ag =961°C
Melting point of Cu =1083°C ,
Eutectic tempreture =780°C
Eutectic compostion =28%Cu
Max solubility of Cu in Ag=9% at 780°C
max.solubilty of c in Ag =2%at 0°C
Max.solubilty of Cu in Ag =9% at 780°c
Max.solubilty of cu in Ag =0% at 0°C.
Detemine the following ;
solidfication start and end solid tempreture for 30% Ag alloy.
TEmpreture at which a 15% Cu alloy has 50% liquid phase and 50% solid phase
Percentage composition of liquid and solid phase 20% Ag alloy at 900°C(10 marks)
6 (a) Draw the TTT digram of austentie for eutectoid steel.Explain the various trasnsmission product of austenite(8 marks)
6 (b) Discuss the process tempreture range range,microstructure of products and application of stress relif annealing(6 marks)
6 (c) Expalin with neat sketch induction hardening process(6 marks)
7 (a) Give the compostion,structure and their application of
S.G iron
Malleable Iron
Gray cast Iron(8 marks)
7 (b) Name at least four important copper base alloys.Give Compostition microstructure and their application (8 marks)
7 (c) Write a note on AL-Si alloys(4 marks)
8 (a) Explain the term composite material with example.State their advantages limitation of composites in practice(8 marks)
8 (b) Usin neat sketch ,explain the process of preparation of metal matrix composite using melting and casting method(8 marks)
8 (c) What are FRPs?Give at least four example(4 marks)